How to control the color difference of injection blow moldin

How to control the color difference of injection blow moldin

Release Time:2020-01-06

Chromatic aberration is a common defect in injection molding. It is not uncommon for injection molding machines to be discarded in batches due to the difference in color of matching parts. There are many factors affecting color difference,...

MORE>
How to solve the plastic shrinkage problem in Dongguan blow

How to solve the plastic shrinkage problem in Dongguan blow

Release Time:2020-01-06

Plastic processing shrinkage of blow molded products is one of the most common problems in plastic processing. For plastic products with high surface quality requirements, shrinkage is even more difficult. Therefore, with the continuous imp...

MORE>
Methods to avoid defects in injection blow moulded products

Methods to avoid defects in injection blow moulded products

Release Time:2020-01-06

In order to obtain high quality injection blow molding products, product engineers must fully consider the product structure and processability when designing products. In the following, we will share some methods to avoid the defects of in...

MORE>
Causes of fading of blow molded products

Causes of fading of blow molded products

Release Time:2020-01-06

Blow molded products, also known as hollow blow molded products, is a rapidly developing plastic processing method. The tubular plastic parison obtained by extrusion or injection molding of a thermoplastic resin is placed in a split mold wh...

MORE>
Precautions for use of Dongguan blow molding equipment

Precautions for use of Dongguan blow molding equipment

Release Time:2020-01-06

1. Before using the blow molding equipment, please read the instruction manual of the injection molding machine used, understand the structure and transmission process of each machine, understand the use of the related control components an...

MORE>
Introduction of wall thickness requirements for plastic part

Introduction of wall thickness requirements for plastic part

Release Time:2020-01-06

The wall thickness of plastic parts processing has a great impact on quality. If the wall thickness is too small and the flow resistance is large, it is difficult for large and complex plastic parts to fill the cavity. The dimensions of the...

MORE>